UNS R56400

Titanium Grade 5 Nylon-insert lock nuts

ISO 7040ASTM B348

Titanium Grade 5 nylon-insert nuts combine a specified alloy body with polymer-generated prevailing torque. Insert temperature, chemical compatibility and reuse performance define the complete nut’s service, including when the body is selected for higher strength than commercially pure titanium at low density.

MOQ
100PCS
Samples · typical
~20 days
Production · typical
25–35 days
Heat treatment
Annealed

EN 10204 3.1 MTC + heat-number traceability

Upload drawing

Which standard is on your order?

Raw Material Specifications

Threads · Metric

Threads · Inch

Dimension Reference

Heat Treatment

Annealed

Annealing reduces working stresses and restores ductility, with atmosphere and surface control limiting contamination during heating.

What we can make in Titanium Grade 5

Nylon locking ring section above metal thread

Nylon insert

Use where a prevailing-torque nut helps retain an adjustment or mounting connection without a separate locking part. The bolt must engage through the nylon ring for the insert to act.

Metal nut body and bearing face

Metal body

The metal threads carry the axial clamp load. Select the body pattern and strength for that load, then check the additional running torque from the insert when setting the tightening process.

Polymer insert separate from alloy body

Temperature & chemicals

Choose this form for equipment temperatures and chemicals compatible with the insert. A nickel-alloy body does not make nylon suitable for furnace service; use an all-metal locking arrangement for elevated-temperature joints.

Locking element
Nylon insert
Drive
External hex
Threads
Metric · Inch
Service limit
Controlled by the insert
Final condition
Annealed
Inspection
Insert retention · Prevailing torque · Dimensions

Manufacturing route

Small lots use machined blanks. Volume nut blanks use a forming route compatible with the alloy before machining the bore and tapping.

Heat treatment & final condition

Forming and thermal processing require contamination control. The final surface is cleaned before dimensional and material acceptance.

Finished geometry

The nylon insert is installed after metal heat treatment and finishing. Prevailing torque is checked on the complete nut, including the specified reuse requirement.

Where Titanium Grade 5 fits — and what matters

Orange welding robot beside a steel fabrication clamped to a workshop positioning table

Industrial Machinery & Automation

Machine frames and positioning fixtures

Titanium Grade 5 nylon-insert lock nuts retain the threaded mountings on machine frames and positioning fixtures using insert-generated prevailing torque. The nylon insert defines the temperature and reuse limits of the complete nut. Alignment, operating cycles and replacement access define the working interface.

Insert temperature · prevailing torque · reuse cycles
Industrial Machinery & Automation fasteners
White centrifugal pump with a bolted casing, black inlet hose and worn paint

Pumps, Valves & OEM

Actuator mounts and pump baseplates

Titanium Grade 5 nylon-insert lock nuts retain the threaded mountings on actuator mounts and pump baseplates using insert-generated prevailing torque. The nylon insert defines the temperature and reuse limits of the complete nut. Repeated maintenance makes fit, engagement and access part of the component specification.

Insert temperature · prevailing torque · reuse cycles
Pumps, Valves & OEM fasteners
Two yellow welding robots working beside a long steel beam fixture in a manufacturing cell

Automotive & EV Manufacturing Equipment

Assembly fixtures and test-rig frames

Titanium Grade 5 nylon-insert lock nuts retain the threaded mountings on assembly fixtures and test-rig frames using insert-generated prevailing torque. The nylon insert defines the temperature and reuse limits of the complete nut. Repeated tooling changes require consistent seating and repeatable assembly dimensions.

Insert temperature · prevailing torque · reuse cycles
Automotive & EV Manufacturing Equipment fasteners

Same nylon-insert lock nut. Different material priorities.

Titanium Grade 5 material data
UNS R50400

Titanium Grade 2

Low mass, corrosion resistance and commercially pure titanium formability.

Connection priority
Metal-body load capacity and polymer-generated prevailing torque
Commercially pure titanium
The Titanium Grade 2 body and the nylon insert need separate acceptance. Cleaner, moisture and temperature exposure reach the insert at the mating thread; its rated condition controls prevailing-torque service.
Titanium Grade 2 nylon-insert lock nuts
UNS N07718

Inconel 718

Precipitation-hardened strength for compact, highly loaded connections.

Connection priority
Metal-body load capacity and polymer-generated prevailing torque
Strength after aging
The Inconel 718 body and the nylon insert need separate acceptance. Cleaner, moisture and temperature exposure reach the insert at the mating thread; its rated condition controls prevailing-torque service.
Inconel 718 nylon-insert lock nuts

From drawing to documented delivery

Heat treatment
Heat treatment
CNC machining
CNC machining
Rockwell hardness testing
Rockwell hardness testing
Wooden-crate packing
Wooden-crate packing
  1. 01Drawing & BOMForm, dimensions and quantity
  2. 02Material & formingGrade, heat and manufacturing route
  3. 03Final inspectionGeometry, threads and ordered tests
  4. 04Documents & dispatchLot records and identified packing

Order documents

Material identity
UNS R56400 · heat number · ordered condition
Final-part acceptance
Grade chemistry, surface condition and the ordered mechanical requirements. Insert identity and complete-nut prevailing-torque results.
Dimensional record
Insert retention · Prevailing torque · Dimensions
Traceability
EN 10204 3.1 material certificate · production lot · identified packing

Build your Titanium Grade 5 nylon-insert lock nut enquiry

QUOTE LIST ITEMTitanium Grade 5 nylon-insert lock nuts; UNS R56400; Nylon-insert lock nut

Questions about Titanium Grade 5 nylon-insert lock nuts

Can a heat-resistant body make the nylon nut suitable for a hot joint?

The nylon remains the temperature-limiting part. Use the actual insert rating and required prevailing-torque performance; a hot-service metal grade does not extend the polymer’s limit.

Technical references & photo credits