UNS N08810

Incoloy 800H Nylon-insert lock nuts

ISO 7040ASTM B408

Incoloy 800H nylon-insert nuts combine a specified alloy body with polymer-generated prevailing torque. Insert temperature, chemical compatibility and reuse performance define the complete nut’s service, including when the body is selected for controlled-carbon, coarse-grain performance for creep duty.

MOQ
100PCS
Samples · typical
~20 days
Production · typical
25–35 days
Heat treatment
Solution annealed

EN 10204 3.1 MTC + heat-number traceability

Upload drawing

Which standard is on your order?

Raw Material Specifications

Threads · Metric

Threads · Inch

Dimension Reference

Heat Treatment

Solution annealed

The specified solution treatment develops the controlled grain structure needed for sustained high-temperature creep duty.

What we can make in Alloy 800H

Nylon locking ring section above metal thread

Nylon insert

Use where a prevailing-torque nut helps retain an adjustment or mounting connection without a separate locking part. The bolt must engage through the nylon ring for the insert to act.

Metal nut body and bearing face

Metal body

The metal threads carry the axial clamp load. Select the body pattern and strength for that load, then check the additional running torque from the insert when setting the tightening process.

Polymer insert separate from alloy body

Temperature & chemicals

Choose this form for equipment temperatures and chemicals compatible with the insert. A nickel-alloy body does not make nylon suitable for furnace service; use an all-metal locking arrangement for elevated-temperature joints.

Locking element
Nylon insert
Drive
External hex
Threads
Metric · Inch
Service limit
Controlled by the insert
Final condition
Solution annealed
Inspection
Insert retention · Prevailing torque · Dimensions

Manufacturing route

Small lots use machined blanks. Volume nut blanks use a forming route compatible with the alloy before machining the bore and tapping.

Heat treatment & final condition

The final solution-treated condition and grain-size requirement are recorded for the ordered H or HT grade. Final dimensions are inspected after the last thermal operation.

Finished geometry

The nylon insert is installed after metal heat treatment and finishing. Prevailing torque is checked on the complete nut, including the specified reuse requirement.

Where 800H fits — and what matters

Orange welding robot beside a steel fabrication clamped to a workshop positioning table

Industrial Machinery & Automation

Machine frames and positioning fixtures

Incoloy 800H nylon-insert lock nuts retain the threaded mountings on machine frames and positioning fixtures using insert-generated prevailing torque. The nylon insert defines the temperature and reuse limits of the complete nut. Alignment, operating cycles and replacement access define the working interface.

Insert temperature · prevailing torque · reuse cycles
Industrial Machinery & Automation fasteners
Two yellow welding robots working beside a long steel beam fixture in a manufacturing cell

Automotive & EV Manufacturing Equipment

Assembly fixtures and test-rig frames

Incoloy 800H nylon-insert lock nuts retain the threaded mountings on assembly fixtures and test-rig frames using insert-generated prevailing torque. The nylon insert defines the temperature and reuse limits of the complete nut. Repeated tooling changes require consistent seating and repeatable assembly dimensions.

Insert temperature · prevailing torque · reuse cycles
Automotive & EV Manufacturing Equipment fasteners
White centrifugal pump with a bolted casing, black inlet hose and worn paint

Pumps, Valves & OEM

Actuator mounts and pump baseplates

Incoloy 800H nylon-insert lock nuts retain the threaded mountings on actuator mounts and pump baseplates using insert-generated prevailing torque. The nylon insert defines the temperature and reuse limits of the complete nut. Repeated maintenance makes fit, engagement and access part of the component specification.

Insert temperature · prevailing torque · reuse cycles
Pumps, Valves & OEM fasteners

Same nylon-insert lock nut. Different material priorities.

Incoloy 800H material data

Incoloy 800

UNS N08800
Carbon
≤0.10%
What changes
General heat and oxidation resistance; no grain-size requirement in the family comparison.
Incoloy 800 nylon-insert lock nuts

Incoloy 800H

UNS N08810 · Current grade
Carbon
0.05–0.10%
What changes
Controlled carbon and coarse-grain condition for creep and stress-rupture duty.

Incoloy 800HT

UNS N08811
Carbon
0.06–0.10%
What changes
Tighter carbon and Al + Ti control (0.85–1.20%), with solution treatment and coarse grain for creep duty.
Incoloy 800HT nylon-insert lock nuts

From drawing to documented delivery

Heat treatment
Heat treatment
CNC machining
CNC machining
Rockwell hardness testing
Rockwell hardness testing
Wooden-crate packing
Wooden-crate packing
  1. 01Drawing & BOMForm, dimensions and quantity
  2. 02Material & formingGrade, heat and manufacturing route
  3. 03Final inspectionGeometry, threads and ordered tests
  4. 04Documents & dispatchLot records and identified packing

Order documents

Material identity
UNS N08810 · heat number · ordered condition
Final-part acceptance
UNS grade, carbon and alloy chemistry, solution-treatment record and ordered grain-size evidence. Insert identity and complete-nut prevailing-torque results.
Dimensional record
Insert retention · Prevailing torque · Dimensions
Traceability
EN 10204 3.1 material certificate · production lot · identified packing

Build your 800H nylon-insert lock nut enquiry

QUOTE LIST ITEMIncoloy 800H nylon-insert lock nuts; UNS N08810; Nylon-insert lock nut

Questions about 800H nylon-insert lock nuts

Can a heat-resistant body make the nylon nut suitable for a hot joint?

The nylon remains the temperature-limiting part. Use the actual insert rating and required prevailing-torque performance; a hot-service metal grade does not extend the polymer’s limit.