UNS N05500 · W.Nr. 2.4375

Monel K-500 Belleville disc springs

EN 16983ISO 6208

Monel K-500 disc springs put age-hardened strength in the nickel–copper alloy family into a flexing preload element. Working force, installed height and final material condition define the part more usefully than free diameter alone.

MOQ
100PCS
Samples · typical
~20 days
Production · typical
25–35 days
Heat treatment
Annealed / age hardened

EN 10204 3.1 MTC + heat-number traceability

Upload drawing
Other alloysX-750718625A-286

Which standard is on your order?

Raw Material Specifications

Dimension Reference

Heat Treatment

Annealed or age hardened

Annealing provides a workable starting condition, while controlled aging develops the higher strength specified for age-hardened K-500.

What we can make in Monel K-500

single disc spring arrangement, axial section

Single disc

Use under a fastener or in a preload mechanism when a short axial space must provide spring force. Select by load at working deflection, not by bore and outside diameter alone.

series disc spring arrangement, axial section

Series stack

Alternate disc orientation when a joint needs more travel to accommodate thermal movement or seating loss. Total travel increases at approximately the single-disc load; guides keep the stack aligned.

parallel disc spring arrangement, axial section

Parallel stack

Nest discs in the same orientation when the available travel is small but more spring force is needed. Load rises at approximately the single-disc deflection, with friction affecting the real load-deflection response.

Form
Conical disc
Key dimensions
Bore · Outside diameter · Thickness
Spring definition
Free height · Load–deflection
Stacking
Single · Series · Parallel
Final condition
Annealed · age hardened
Inspection
Free height · Thickness · Load–deflection

Manufacturing route

Disc blanks are cut and formed to the required cone height; thickness and edge quality control stress distribution through the working travel.

Heat treatment & final condition

Solution treatment and the specified aging condition are recorded against the production lot; final dimensions are checked after thermal processing.

Working performance

The spring heat-treatment condition is selected for working stress and temperature. Load at working deflection and permanent set are acceptance characteristics.

Where K-500 fits — and what matters

Ship machinery compartment with green pumps, insulated pipes and pressure gauges

Offshore & Marine

Deck-equipment brackets and marine pump skids

Monel K-500 disc spring / belleville washers form preload stacks in the bolted mounts of deck-equipment brackets and marine pump skids. Working deflection allows the stack to accommodate movement while maintaining the designed spring force. The assembled contact is exposed to saltwater, deposits and neighbouring metals.

Stack arrangement · working deflection · load retention
Offshore & Marine fasteners
Water-treatment machinery with parallel green pipes, gray pumps and yellow access platforms

Water Treatment & Desalination

Membrane-skid and pump supports

Monel K-500 disc spring / belleville washers form preload stacks in the bolted mounts of membrane-skid and pump supports. Working deflection allows the stack to accommodate movement while maintaining the designed spring force. The water stream, cleaning cycle and retained liquid define exposure at the installed part.

Stack arrangement · working deflection · load retention
Water Treatment & Desalination fasteners
Gas-processing plant with a process tower and twin stacks beyond a cultivated field

Oil & Gas

Utility skids and instrument supports

Monel K-500 disc spring / belleville washers form preload stacks in the bolted mounts of utility skids and instrument supports. Working deflection allows the stack to accommodate movement while maintaining the designed spring force. Utility connections and pressure-boundary parts have separate acceptance requirements on the equipment drawing.

Stack arrangement · working deflection · load retention
Oil & Gas fasteners

Same disc spring. Different material priorities.

Monel K-500 material data
UNS N07750

Inconel X-750

Age-hardened strength and a choice of hot-service heat treatments.

Connection priority
Force at working deflection and relaxation during dwell
Spring treatment versus bolting treatment
X-750 has several heat-treatment routes. The route for retained spring force is selected around relaxation and working stress; a bolting strength requirement calls for its own specified condition. At the loaded disc faces and stack contact edges, the relevant metal temperature can differ from the process or furnace set point.
Inconel X-750 disc spring / belleville washers
UNS N07718

Inconel 718

Precipitation-hardened strength for compact, highly loaded connections.

Connection priority
Force at working deflection and relaxation during dwell
Strength after aging
Machine-stock properties and final aged properties describe different states. The final heat-treatment lot and mechanical results establish the strength available in the installed part. At the loaded disc faces and stack contact edges, the relevant metal temperature can differ from the process or furnace set point.
Inconel 718 disc spring / belleville washers
UNS N06625

Inconel 625

Solid-solution strength and resistance to aggressive process liquids.

Connection priority
Force at working deflection and relaxation during dwell
Annealed or solution-annealed 625
The delivery condition affects strength and high-temperature response. Keep the specified condition with the component’s mechanical acceptance; 718-style aging is not the strengthening route for 625. Include liquid retained at the loaded disc faces and stack contact edges in the exposure description.
Inconel 625 disc spring / belleville washers

From drawing to documented delivery

Heat treatment
Heat treatment
CNC machining
CNC machining
Rockwell hardness testing
Rockwell hardness testing
Wooden-crate packing
Wooden-crate packing
  1. 01Drawing & BOMForm, dimensions and quantity
  2. 02Material & formingGrade, heat and manufacturing route
  3. 03Final inspectionGeometry, threads and ordered tests
  4. 04Documents & dispatchLot records and identified packing

Order documents

Material identity
UNS N05500 · heat number · ordered condition
Final-part acceptance
Lot-linked aging record and mechanical acceptance in the final condition. Load–deflection and permanent-set results for the specified spring geometry.
Dimensional record
Free height · Thickness · Load–deflection
Traceability
EN 10204 3.1 material certificate · production lot · identified packing

Build your K-500 disc spring enquiry

QUOTE LIST ITEMMonel K-500 disc spring / belleville washers; UNS N05500; Single disc

Questions about K-500 disc spring / belleville washers

Can an alloy change preserve the same disc-spring rating?

Elastic modulus, yield behaviour and final condition influence the load–deflection curve. Recalculate and verify the working response for the selected alloy rather than carrying over a same-size steel disc’s rating.

Technical references & photo credits