Material selection

Compare Materials

Choose up to three materials. Compare their properties, reference conditions and specification requirements side by side.

47 matching materials

Nickel AlloysUNS N06625View material details
Nickel AlloysUNS N07718View material details

Scroll horizontally to compare all columns.

Compare Materials: Inconel 625, Inconel 718
MaterialInconel 625N06625Inconel 718N07718

Summary

Material familyNickel AlloysNickel Alloys
Grade / UNSN06625N07718
SummaryA solid-solution-strengthened nickel alloy used in marine and chemical-processing equipment.An age-hardenable nickel alloy for fasteners and components requiring strength and corrosion resistance.

Performance overview

Material focusStrength without an aging treatmentStrength developed through aging
Physical reference
Density
8.44 g/cm³
Melting range
1290–1350 °C
Supplied technical reference · Scanned PDF page 12 · printed page 24
Density
8.19 g/cm³
Melting range
1260–1336 °C
Supplied technical reference · Scanned PDF page 12 · printed page 24
Chemical composition
Chemical composition

Composition limits · wt.%

Ni
≥58
Cr
20–23
Mo
8–10
Nb + Ta
3.15–4.15
Fe
≤5
C
≤0.10
Mn
≤0.50
Si
≤0.50
P
≤0.015
S
≤0.015
Al
≤0.40
Ti
≤0.40
Co (if determined)
≤1.0
Special Metals · Alloy 625 · Tables 1, 2 & 5; Available Products and Specifications (page 17) ↗
Chemical composition

Composition limits · wt.%

Ni
50–55
Cr
17–21
Nb + Ta
4.75–5.50
Mo
2.80–3.30
Ti
0.65–1.15
Al
0.20–0.80
Fe
Balance
C
≤0.08
Mn
≤0.35
Si
≤0.35
P
≤0.015
S
≤0.015
B
≤0.006
Cu
≤0.30
Co
≤1.0
Supplied technical reference · Scanned PDF page 4 · printed page 16

Mechanical properties

Reference conditions vary or are incomplete. Read the basis, condition and source for each column; these values do not establish a performance ranking or finished-fastener acceptance values.

Tensile strength724–896 MPa
Nominal reference range
Solution treated
Room temperature
Special Metals · Alloy 625 · Tables 1, 2 & 5; Available Products and Specifications (page 17) ↗
1389 MPa
Typical reference sample
Annealed + aged
Room temperature
Special Metals · Alloy 718 · SMC-045, September 2007 · Tables 1 & 8 ↗
0.2% yield strength290–414 MPa
Nominal reference range
Solution treated
Room temperature
Special Metals · Alloy 625 · Tables 1, 2 & 5; Available Products and Specifications (page 17) ↗
1207 MPa
Typical reference sample
Annealed + aged
Room temperature
Special Metals · Alloy 718 · SMC-045, September 2007 · Tables 1 & 8 ↗
Elongation40–65 %
Nominal reference range
Solution treated
Room temperature
Special Metals · Alloy 625 · Tables 1, 2 & 5; Available Products and Specifications (page 17) ↗
20 %
Typical reference sample
Annealed + aged
Room temperature
Special Metals · Alloy 718 · SMC-045, September 2007 · Tables 1 & 8 ↗
Reference conditions
Data basis
Nominal reference range
Condition
Solution treated
Sample form
Rod, bar & plate
Sample size
Up to 101.6 mm
Test temperature
Room temperature
Test method
Not documented in this reference
Test direction
Not documented in this reference
Elongation gauge length
Not documented in this reference
Data basis
Typical reference sample
Condition
Annealed + aged
Sample form
Hot-rolled bar · Ø25.4 mm
Sample size
1.0 in diameter (25.4 mm)
Test temperature
Room temperature
Test method
Not documented in this reference
Test direction
Longitudinal
Elongation gauge length
Not documented in this reference

Temperature & corrosion

Evaluate the medium, concentration, impurities, temperature and loading together. A melting point or oxidation reference is not a safe working-temperature limit.

Service conditions to reviewMatch the annealed or solution-treated condition to the application.Specify the heat treatment and strength requirement.
Temperature-dependent data
  • Strength and elongation vs temperatureHot-rolled plate · mill annealed at 1052°C
View material details
  • Strength and elongation vs temperaturePlate · mill annealed + aged
View material details

Heat treatment

Delivery condition and heat-treatment requirements are agreed for the requested product form and order.

ConditionSolution treatedAnnealed + aged
Reference treatmentNot documented in this reference1750°F / 1 h, then 1325°F / 8 h; furnace cool to 1150°F for 18 h total aging.Special Metals · Alloy 718 · SMC-045, September 2007 · Tables 1 & 8 ↗

Reference applications

Application examples provide context for review; suitability depends on the actual service conditions.

Reference applicationsSeawater equipment · chemical-process valves & heat exchangersGas-turbine assemblies · cryogenic equipment

Standards & documentation

Confirm the edition, product form and condition. Material specifications do not establish finished-fastener compliance.

Material specifications by form
Sources
Sources
Sources

Documents for your enquiry

Every BYBOLT delivery includes an MTC / EN 10204 3.1 certificate, heat-number traceability and mechanical testing. Threaded products include sampled GO / NO-GO gauging. Test methods and acceptance criteria follow the agreed specification; PMI, third-party inspection and additional records are agreed separately at quotation.

Take your shortlist to the next step

Share your drawing or product form, dimensions, quantity and operating conditions. Your selected materials will be included as alternatives for review.

Get a Quote