MaterialHastelloy C-276N10276Hastelloy C-22N06022

Summary

Material familyNickel AlloysNickel Alloys
Grade / UNSN10276N06022
SummaryA nickel-chromium-molybdenum alloy used in corrosive chemical environments.A nickel-chromium-molybdenum alloy for equipment exposed to aggressive chemical media.

Performance overview

Material focusResistance in aggressive chemical mediaResistance to localized corrosion
Physical reference
Density
8.89 g/cm³
Melting range
1325–1370 °C
Supplied technical reference · Scanned PDF page 11 · printed page 23
Not documented in this reference
Chemical composition
Chemical composition

Composition limits · wt.%

Ni
Balance
Cr
14.5–16.5
Mo
15–17
Fe
4–7
W
3–4.5
Co
≤2.5
C
≤0.01
Mn
≤1.0
P
≤0.04
S
≤0.03
Si
≤0.08
V
≤0.35
Supplied technical reference · Scanned PDF page 6 · printed page 18
Chemical composition

Composition limits · wt.%

Ni
Balance
Cr
20–22.5
Mo
12.5–14.5
Fe
2–6
W
2.5–3.5
Co
≤2.5
C
≤0.015
Mn
≤0.50
P
≤0.02
S
≤0.02
Si
≤0.08
V
≤0.35
Supplied technical reference · Scanned PDF page 6 · printed page 18

Mechanical properties

Reference conditions vary or are incomplete. Read the basis, condition and source for each column; these values do not establish a performance ranking or finished-fastener acceptance values.

Tensile strength792 MPa
Published reference sample
Mill annealed
Room temperature
Haynes · C-276 · Nominal Composition; Tensile Strength and Elongation; Resistance to Pitting and Crevice Corrosion ↗
≥690 MPa
Catalogue reference minimums
Not documented in this reference
Not documented in this reference
Supplied technical reference · Scanned PDF page 6 · printed page 18
0.2% yield strength356 MPa
Published reference sample
Mill annealed
Room temperature
Haynes · C-276 · Nominal Composition; Tensile Strength and Elongation; Resistance to Pitting and Crevice Corrosion ↗
≥310 MPa
Catalogue reference minimums
Not documented in this reference
Not documented in this reference
Supplied technical reference · Scanned PDF page 6 · printed page 18
Elongation61 %
Published reference sample
Mill annealed
Room temperature
Haynes · C-276 · Nominal Composition; Tensile Strength and Elongation; Resistance to Pitting and Crevice Corrosion ↗
≥45 %
Catalogue reference minimums
Not documented in this reference
Not documented in this reference
Supplied technical reference · Scanned PDF page 6 · printed page 18
Reference conditions
Data basis
Published reference sample
Condition
Mill annealed
Sample form
Sheet · 2 mm thickness
Sample size
0.078 in (2 mm) sheet
Test temperature
Room temperature
Test method
Not documented in this reference
Test direction
Not documented in this reference
Elongation gauge length
Not documented in this reference
Data basis
Catalogue reference minimums
Condition
Not documented in this reference
Sample form
Not documented in this reference
Sample size
Not documented in this reference
Test temperature
Not documented in this reference
Test method
Not documented in this reference
Test direction
Not documented in this reference
Elongation gauge length
A5, as labelled in supplied table

Temperature & corrosion

Evaluate the medium, concentration, impurities, temperature and loading together. A melting point or oxidation reference is not a safe working-temperature limit.

Service conditions to reviewCheck the actual medium, concentration and temperature.Review the exact medium, concentration and temperature.
Temperature-dependent data
  • Strength and elongation vs temperatureAnnealed material · supplied reference
View material details
Not documented in this reference

Heat treatment

Delivery condition and heat-treatment requirements are agreed for the requested product form and order.

ConditionMill annealedNot documented in this reference
Reference treatmentMill-annealed wrought material context; no heat cycle is attached to this tensile row.Haynes · C-276 · Nominal Composition; Tensile Strength and Elongation; Resistance to Pitting and Crevice Corrosion ↗Not documented in this reference

Reference applications

Application examples provide context for review; suitability depends on the actual service conditions.

Reference applicationsChemical-process equipment · heat exchangersChemical-process equipment · flue-gas desulfurization

Standards & documentation

Confirm the edition, product form and condition. Material specifications do not establish finished-fastener compliance.

Material specifications by form
Sources
Sources
Sources

Documents for your enquiry

Every BYBOLT delivery includes an MTC / EN 10204 3.1 certificate, heat-number traceability and mechanical testing. Threaded products include sampled GO / NO-GO gauging. Test methods and acceptance criteria follow the agreed specification; PMI, third-party inspection and additional records are agreed separately at quotation.

Take your shortlist to the next step

Share your drawing or product form, dimensions, quantity and operating conditions. Your selected materials will be included as alternatives for review.

Get a Quote
Get a Quote