| Material | Alloy 926N08926 | 254 SMOS31254 |
|---|---|---|
Summary | ||
| Material family | Special Stainless & Iron-Base Alloys | Special Stainless & Iron-Base Alloys |
| Grade / UNS | N08926 | S31254 |
| Summary | A high-alloy austenitic stainless steel with molybdenum and nitrogen for chloride-bearing environments. | A high-molybdenum austenitic stainless steel used in chloride-bearing process environments. |
Performance overview | ||
| Material focus | 6Mo austenitic stainless | 6Mo austenitic stainless |
| Physical reference | Not documented in this reference | Not documented in this reference |
| Chemical composition | Chemical compositionSelected composition limits · wt.%
| Chemical compositionComposition limits · wt.%
|
Mechanical propertiesReference conditions vary or are incomplete. Read the basis, condition and source for each column; these values do not establish a performance ranking or finished-fastener acceptance values. | ||
| Tensile strength | 600–800 MPa Published specified limits VDM Metals · Alloy 926 · April 2024 · Tables 2 & 5 ↗Solution annealed Room temperature | ≥650 MPa Catalogue reference minimums Supplied technical reference · Scanned PDF page 2 · printed page 14Not documented in this reference Not documented in this reference |
| 0.2% yield strength | ≥300 MPa Published specified limits VDM Metals · Alloy 926 · April 2024 · Tables 2 & 5 ↗Solution annealed Room temperature | ≥300 MPa Catalogue reference minimums Supplied technical reference · Scanned PDF page 2 · printed page 14Not documented in this reference Not documented in this reference |
| Elongation | ≥40 % Published specified limits VDM Metals · Alloy 926 · April 2024 · Tables 2 & 5 ↗Solution annealed Room temperature | ≥35 % Catalogue reference minimums Supplied technical reference · Scanned PDF page 2 · printed page 14Not documented in this reference Not documented in this reference |
| Reference conditions |
|
|
Temperature & corrosionEvaluate the medium, concentration, impurities, temperature and loading together. A melting point or oxidation reference is not a safe working-temperature limit. | ||
| Service conditions to review | Specify solution-annealed condition and the relevant product dimensions. | Check crevices, chloride concentration and temperature. |
| Temperature-dependent data | Not documented in this reference | Not documented in this reference |
Heat treatmentDelivery condition and heat-treatment requirements are agreed for the requested product form and order. | ||
| Condition | Solution annealed | Not documented in this reference |
| Reference treatment | Not documented in this reference | Not documented in this reference |
Reference applicationsApplication examples provide context for review; suitability depends on the actual service conditions. | ||
| Reference applications | Offshore seawater systems · acid-processing equipment | Seawater equipment · chemical-process equipment |
Standards & documentationConfirm the edition, product form and condition. Material specifications do not establish finished-fastener compliance. | ||
| Material specifications by form |
|
|
| Sources | Sources
| |
Documents for your enquiry
Every BYBOLT delivery includes an MTC / EN 10204 3.1 certificate, heat-number traceability and mechanical testing. Threaded products include sampled GO / NO-GO gauging. Test methods and acceptance criteria follow the agreed specification; PMI, third-party inspection and additional records are agreed separately at quotation.
Take your shortlist to the next step
Share your drawing or product form, dimensions, quantity and operating conditions. Your selected materials will be included as alternatives for review.